Silicon calcium manganese deoxidizer

HOME > News
Silicon-calcium-manganese deoxidizer is a new type of composite deoxidizer with better deoxidation effect in steelmaking production. The existing silicon-calcium-manganese deoxidizer is smelted in an induction furnace. Because the raw material used is metal manganese or alloy (silicon-calcium alloy) first smelted from ore, and then smelted for the second time. Therefore the production process is loaded down with trivial details, and energy consumption is big, and cost is high, affects the price of product. In particular, the main raw material, metal manganese, is expensive. Once the market is in short supply, it will directly affect the production of silicon-calcium-manganese deoxidizers.

The new silicon-calcium-manganese deoxidizer is a kind of ore containing silicon, calcium and manganese as raw materials, which is smelted into a silicon-calcium-manganese deoxidizer by selecting an appropriate formula to replace the raw materials such as metal manganese and silicon-calcium in the existing production method. , which simplifies the production process, which can save energy and reduce production costs.

The silicon-calcium-manganese deoxidizer uses ore rich in silicon, calcium and manganese as the main raw material, and is smelted into a silicon-calcium-manganese deoxidizer in a submerged arc furnace at one time. The process steps are as follows: mechanically crush the raw materials such as silica, pick out impurities, It is fully mixed with coke powder, coal, and steel scraps, and then fed into the submerged arc furnace for smelting. The smelting temperature is 1700 ° C ~ 2000 ° C. After testing, the chemical composition content (weight) silicon (Si) 20-55%, calcium (Al ) 20-30%, manganese (Ba) 6-8% silicon calcium manganese deoxidizer.

The silicon-calcium-manganese deoxidizer has been tested for deoxidation in steelmaking and shows that it has achieved a good deoxidation effect. It directly selects ores containing silicon, calcium, and manganese as raw materials. The time for secondary smelting with alloys reduces the waste of labor and energy and the defects of low production efficiency. Therefore, compared with the existing production method, it not only reduces the smelting procedure, but also has the characteristics of simple method, low energy consumption, labor saving and low cost.
Contact Us Today!
We welcome inquiries in English, Español (Spanish), Русский язык (Russian), Français (French), and العربية (Arabic). Our professional team will reply to you within one business day. Please feel FREE to contact us!
Your privacy is important to us,we are committed to marking sure your privacy is confidential.
Top